r/AdditiveManufacturing
What is the standard average nesting density you run in SLS? How you manage the heat?
- upvotes
- 7
- comments
- 6
Post
Hey all, I run an EOS P396 with PA12 and I'm trying to see how other shops handle this. We keep nesting around 7-8%. Anything higher and the powder seems to degrade way faster. With a 70/30 (used/virgin) refresh, we get about 8-10 cycles from the dry run phase. After that, orange peel starts showing up and it's hard to shake. So I'm curious: What density do you usually run on average? If you go higher, how do you handle the heat? Spacing, cooling time, temp tweaks? What refresh ratio do you use, and how many cycles before you boost virgin or dump? Has anyone changed settings to get more density without wrecking the powder? Would love to hear what's working for you, even rough numbers. Thanks!
Extracted from these lines
[comment u/jaydengallagher] Pack at 15-20% density 2mm model spacing. Using the Formlabs fuse 1+. Though none of our parts are very thick normally between 2.5mm to 5mm so no solid geometry causing warping to neighbouring parts.
[comment u/jaydengallagher] This is using nylon 11 at 30% fresh powder and No2 chamber. Having refresh so close to packing density it will be close to 30 runs before we give it a fresh boost of powder.